Recommended Practice for Concrete Inspection

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommended Practice for Concrete Inspection

Author(s): ACI Committee 311

Publication: Journal Proceedings

Volume: 60

Issue: 11

Appears on pages(s): 1525-1534

Keywords:

DOI: 10.14359/7903

Date: 11/1/1963

Abstract:
This recommended practice sets forth standards and procedures relating to concrete construction which will serve as a guide to owners, architects, and engineers in planning their inspection pro as a requirement Program. The need for adequate inspection or high quality, attractive appearing concrete at the least cost is emphasized.