Admixtures for Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Admixtures for Concrete

Author(s): ACI Committee 212

Publication: Journal Proceedings

Volume: 60

Issue: 11

Appears on pages(s): 1481-1524

Keywords:

DOI: 10.14359/7902

Date: 11/1/1963

Abstract:
This third report of ACI Committee PIP, Admixtures for Concrete, updates the previous reports of 1944 and 1954. In this report admixtures are classified in 15 groups according to type of materials constituting the admixtures, to the characteristic effects of their use. Where an admixture possesses properties identifiable with more than one group it is discussed with the group that describes its most important effect on concrete. Types of admixtures discussed are: (1) acceleratingi (2) water-reducing and set-controlling; (3) grouting, (4) air-entraining; (5) air-detraining (6) gas-form ing; (7) expansion-producing; (8) finely divided mineral; <9) damp-proofing and permeability-reducing] (10) bonding; (11) alkali-aggregate-expansion-reducing] (19) corrosion-inhibiting; (13) fun icidal germicidal, and insecticidal; (14) flocculating; an j (1 5 ) koloring. An extensive list of references is included.