Title: Investigation of Multiple Panel Reinforced Concrete Floor Slabs

Author(s): Mete A. Sozen and Chester p. Siess

Publication: Journal Proceedings

Volume: 60

Issue: 8

Appears on pages(s): 999-1028

Keywords:

DOI: 10.14359/7888

Date: 8/1/1963

Abstract:
This is the first of a number of reports to be published on an investigation of multiple-panel concrete floor slabs. The paper serves as an introduction to the later reports presenting the historical background of the design methods for floor slabs in ACI 318-56 and the overall results of tests on five structures tested during the investigation.