Analysis and Design of a Cantilever Saircase

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis and Design of a Cantilever Saircase

Author(s): Phillip L. Gould

Publication: Journal Proceedings

Volume: 60

Issue: 7

Appears on pages(s): 881-900

Keywords:

DOI: 10.14359/7883

Date: 7/1/1963

Abstract:
The various factors influencing the behavior of a cantilever staircase are discussed and evaluated. Particular attention is given to the torsional moment at the intermediate landing and the support condition of the upper leg. A design example is presented illustrating those calculations that are peculiar to this type of structure.