Load-Balancing Method for Design and Analysis of Prestressed Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load-Balancing Method for Design and Analysis of Prestressed Concrete Structures

Author(s): T. Y. Lin

Publication: Journal Proceedings

Volume: 60

Issue: 6

Appears on pages(s): 719-742

Keywords:

DOI: 10.14359/7874

Date: 6/1/1963

Abstract:
The concept of load balancing is introduced for pre-stressed concrete structures, as a third approach after the elastic stress and the ultimate strength methods of design and analysis. It is first applied to simple beams and canti-levers and then to continuous beams and rigid frames. Principles of load balancing for flat slabs, grid systems, and certain forms of shells and folded plates are introduced. The amount of loading to be balanced by prestressing ist suggested. Accuracy and limitations of the method are discussed.