Test of Reinforced Concrete Columns with High Slenderness Ratios

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Test of Reinforced Concrete Columns with High Slenderness Ratios

Author(s): Luis P. Saenz and Ignacio Martin

Publication: Journal Proceedings

Volume: 60

Issue: 5

Appears on pages(s): 589-616

Keywords:

DOI: 10.14359/7870

Date: 5/1/1963

Abstract:
Tests were made at the Materials Testing Laboratory of the University of Havana with 59 rectangular section concrete columns having longitudinal reinforcement with ties and flat ends with slenderness ratios varying from 21.6 to 43.0. The results of loads, stresses, and deformations are given and a Rankine type formula is developed based on these, to establish the relation between the strength of short columns and of columns with high slenderness ratios. Using this relation, another Rankine type formula is suggested for practical design of short, intermediate, and long columns. This formula is compared with formulas of the American Concrete Institute, British, German, and Russian codes.