Strength and Deflection of Circular Uniformly Loaded Slab Supported Between Center and Periphery

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength and Deflection of Circular Uniformly Loaded Slab Supported Between Center and Periphery

Author(s): S. Sergev and M. H. Kashani-Sabet

Publication: Journal Proceedings

Volume: 60

Issue: 2

Appears on pages(s): 281-294

Keywords:

DOI: 10.14359/7856

Date: 2/1/1963

Abstract:
Formulas for principal bending moments and deflections are derived for a uniformly loaded circular slab, simply supported by a continuous circular support situated between center and heperiphery of the slab. The bending moments and deflections are found for different positions of the support, and for design purposes, these functions are plotted as ordinates and the location of the support as abscissas, both in nondimensional form. The construction is suitable for roofs of circular structures where an overhana is desirable. The paper does not offer a new solution to the problem but attempts to present it in a suitable form for the designer. The paper is concluded by an example showing the use of the curves presented.