Title: 
            Direct Design of Prestressed Concrete Members
        
        
            Author(s): 
            Kolbjorn Saether
        
        
            
                Publication: 
                Journal Proceedings
            
            
                Volume: 
                60
            
            
                Issue: 
                2
            
            
                Appears on pages(s): 
                239-260
            
            
                Keywords: 
                
            
            
                DOI: 
                10.14359/7854
            
        
        
            Date: 
            2/1/1963
        
        
            Abstract:
            Presents a tool for the design of prestressed concrete members. A series of mathematical derivations are presented showing the step by step procedure from given loads and stresses to the corresponding resulting cross section.  This section is subsequently checked for compliance with the ultimate load requirements. A desian program and adesign example are discussion of its oract ica aoolication. given with a short A long series of modifications to the presented designis possible using the same set of equations free and independently variable section maintained. as long as properties