Recommended Practice for Concrete Formwork

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommended Practice for Concrete Formwork

Author(s): ACI Committee 347

Publication: Journal Proceedings

Volume: 60

Issue: 2

Appears on pages(s): 169-170

Keywords:

DOI: 10.14359/7848

Date: 1/1/1963

Abstract:
Presents brief introductory statement on the need for formwork standards based on the fact that 35 to 60 percent of the total cost of the concrete work in a protect in the United States is in the formwork. A section is given on engineer-architect specifications noting the kind and amount of specification the engineer or architect should provide the contractor. Since the committee concludes that formwork design and engineering as well as construction, must be the responsibility of the contractor, the recommendations contained in the report are directed to that group. However, an understanding of these recommendations by engineers and architects will aid these groups in their specification functions.