Stresses Around Circular Inclusions Due to Thermal Gradients with Particular Reference to Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stresses Around Circular Inclusions Due to Thermal Gradients with Particular Reference to Reinforced Concrete

Author(s): J. Dundurs and 0. C. Zienkiewicz

Publication: Journal Proceedings

Volume: 61

Issue: 12

Appears on pages(s): 1523-1534

Keywords:

DOI: 10.14359/7837

Date: 12/1/1964

Abstract:
A solution of an elastic, conducting circular inclusion in an elastic medium subject to a uniform temperature gradient is presented. The problem has several practical applications, but interest on it was focused by the increasing use of reinforced concrete in situations of high temperature gradients, such as nuclear reactor shields. The magnitude and distribution of stresses around a steel reinforcing bar in concrete is studied in some detail.