Horizontal Shear Connections Between Precast Beams and Cast-in -Place

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Horizontal Shear Connections Between Precast Beams and Cast-in -Place

Author(s): J. C. Saemann and George W. Washa

Publication: Journal Proceedings

Volume: 61

Issue: 11

Appears on pages(s): 1383-1410

Keywords:

DOI: 10.14359/7832

Date: 11/1/1964

Abstract:
This project has been concerned with the strength of the joint between precast concrete beams and cast-in-place concrete slabs. In the experimental program 42 beams and necessary control cylinders were tested in an attempt to provide information on the following variables: degree of roughness of contact surface, length of shear span, percentage of steel across the joint, effect of shear keys, position of the joint with respect to the neutral axis, and concrete compressive strength. Results obtained indicate complex relations between roughness of surface joint, percent steel across joint, and shear span.