Damping Characteristics of Prestressed Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Damping Characteristics of Prestressed Concrete

Author(s): Joseph Penzien

Publication: Journal Proceedings

Volume: 61

Issue: 9

Appears on pages(s): 1125-1148

Keywords:

DOI: 10.14359/7824

Date: 9/1/1964

Abstract:
Reports on an investigation to determine the basic damp ing characteristics of prestressed concrete beams under dynamic loading. The basic structural parameters varied in the experiment were: type of prestress, intensity of prestress, and ultimate strength of concrete. The dynamic conditions imposed on each specimen were steady state forced vibration and free vibration about the static unloaded equilibrium position. Internal damping was observed to depend a great deal on loading history and on amplitude of displacement. was also observed that cracking of concrete is an important parameter. Therefore, magnitude and type of prestress have an indirect influence on damping since they control cracking to a considerable extent. Most of the equivalent viscous damping factors measured ranged, from 0.5 to 7.0 percent of critical values depending on the degree of cracking permitted in each test.