Title: Response o fSingly Reinforced Beams to Cyclic Loading

Author(s): B. P. Sinha, Kurt H. Gerstle and Leonard D. Tulin

Publication: Journal Proceedings

Volume: 61

Issue: 8

Appears on pages(s): 1021-1038

Keywords:

DOI: 10.14359/7819

Date: 8/1/1964

Abstract:
Reports on an investigation of the response of simply supported beams to arbitrary cyclic load histories. A bending theory of reinforced beams is developed and compared with test results. Comparison indicates that the theory may give a rough indication of the behavior of reinforced concrete beams under cyclic loading.