Glossary of Terms on Cement and Concrete Technology-Increment No. 6

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Glossary of Terms on Cement and Concrete Technology-Increment No. 6

Author(s): ACI Committee 116

Publication: Journal Proceedings

Volume: 61

Issue: 8

Appears on pages(s): 913-920

Keywords:

DOI: 10.14359/7813

Date: 8/1/1964

Abstract:
As part of its mission, ACI Committee 116, Nomenclature, represents the fourth published installment of a glossary of terms on cement ond concrete technology. The glossary has been divided into 13 increments which are being pre-sented to elicit discussion as they are completed, regardless of order. Following publication and discussion of the final installment, the committee will review and combine the groups for consideration as an ACI standard.