The Restrained Long Concrete Column as a Part of a Rectangular Frame

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Restrained Long Concrete Column as a Part of a Rectangular Frame

Author(s): John E. Breen and Phil M. Ferguson

Publication: Journal Proceedings

Volume: 61

Issue: 5

Appears on pages(s): 563-588

Keywords:

DOI: 10.14359/7797

Date: 5/1/1964

Abstract:
This investigation was concerned with the long tied column as part of a building frame. The column was directly loaded axially while a beam supplied a moment loading in such a manner that the far end of the column was restrained against rotation, but was not completely fixed. Short-time loading to failure was used for five frames. A single test under 90 day sustained load followed by loading to failure was included. At a nominal eccentricity of 0.3 of the column thickness, there was no long column strength reduction. At an eccentricity of 0.1 of the column thickness there was no long column strength reduction at an h/l of 15 but at an h/t of 30 there was a 3 percent reduction for one speci-men and 8 percent for another. The longer columns were considerably relieved of their moment loading by virtue of their reduced stiffness at higher loads. The shorter columns were greatly shielded by compression hinging at their loaded end.