Construction of a Buttressed Dome Segment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction of a Buttressed Dome Segment

Author(s): Andrew R. Nasser

Publication: Journal Proceedings

Volume: 61

Issue: 5

Appears on pages(s): 509-520

Keywords:

DOI: 10.14359/7794

Date: 5/1/1964

Abstract:
Presents the construction phase of the Culver City High School Auditorium in southern California. Provides a general description of the structure but is principally a descriptive record of the construction operations.