Prefabricated Building Made of Triangular Prestressed Components

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prefabricated Building Made of Triangular Prestressed Components

Author(s): Zenon A. Zielinski

Publication: Journal Proceedings

Volume: 61

Issue: 4

Appears on pages(s): 383-398

Keywords:

DOI: 10.14359/7788

Date: 4/1/1964

Abstract:
Describes a factory building in Warsaw, Poland, where the basic structural element is a precast unit in the shape of an equilateral triangle. The unit was used for both floors and walls. While the building was designed to be prefabricated, it presents all the advantages of a monolithic structure.