Title: On the Formula for Spiral Reinforcement

Author(s): Ti Huang

Publication: Journal Proceedings

Volume: 61

Issue: 3

Appears on pages(s): 351-354

Keywords:

DOI: 10.14359/7786

Date: 3/1/1964

Abstract:
Discusses the ACI Building Code formula for finding the minimum amount of spiral reinforcement in short columns. Suggests a modification of the formula based on data obtained from triaxial tests of concrete.