Title: Equation for the Stress-Strain Curve of Concrete

Author(s): Prakash Desayi and S. Krishnan

Publication: Journal Proceedings

Volume: 61

Issue: 3

Appears on pages(s): 345-350

Keywords:

DOI: 10.14359/7785

Date: 3/1/1964

Abstract:
A simple equation is proposed for the stress-strain curve of concrete in compression. The equation is found to represent it well not only up to the maximum stress but also beyond, and may conveniently be adopted in the computa-tion of ultimate resisting moment of reinforced concrete sections.