Increasing Tensile Strength of Terrazzo

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Increasing Tensile Strength of Terrazzo

Author(s): A. M. Neville

Publication: Journal Proceedings

Volume: 61

Issue: 3

Appears on pages(s): 335-344

Keywords:

DOI: 10.14359/7784

Date: 3/1/1964

Abstract:
Results of tests on terrazzo as normally used and with the addition of glass fiber or asbestos fiber are presented. It is shown that glass fiber improves the early strength of terrazzo made with a moderately rapid hardening cement.