Foundation Bolts for Heavy Drives

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Foundation Bolts for Heavy Drives

Author(s): Chesman A. Lee

Publication: Journal Proceedings

Volume: 61

Issue: 2

Appears on pages(s): 189-194

Keywords:

DOI: 10.14359/7774

Date: 2/1/1964

Abstract:
Discusses the design assumptions for determining the size of the foundation bolts for a heavy drive. Presents simple calculations for finding the moment of resistance, the ten- sions in the bolts, and the pressure on the concrete.