Load-Sharing Precast Concrete Slats

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load-Sharing Precast Concrete Slats

Author(s): Avinadav Siev and Jacob Maos

Publication: Journal Proceedings

Volume: 62

Issue: 12

Appears on pages(s): 1581-1590

Keywords: beam, cattle shed, floor, live load, load sharing, precast concrete, slat

DOI: 10.14359/7763

Date: 12/1/1965

Abstract:
Precast beams used in slatted flooring in cattle sheds were heretofore designed for each to carry the whole widely-varying live load, and are both bulky and expensive as a result. The paper presents a method for linking separate slats with a view to distributing the live load. Tests have shown that this results in sharing of the load, thereby permitting considerable saving in dimensions, weight, and reinforcement.