Prestress Transfer Bond of Pretensioned Strands in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prestress Transfer Bond of Pretensioned Strands in Concrete

Author(s): R. Stanton Over and Tung

Publication: Journal Proceedings

Volume: 62

Issue: 11

Appears on pages(s): 1451-1460

Keywords: beam, bond strength, friction, prestressed concrete, pretensioning, research, strand

DOI: 10.14359/7756

Date: 11/1/1965

Abstract:
Discusses the frictional and mechanical bond of seven-wire strands used in pretensioned concrete. The bond transfer lengths required for strands of l/2, 3/8, and l/4 in. nominal diameters are determined experimentally, and are found to increase considerably for strands of larger diameters.