Slip-Form Lining of the San Luis Canal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Slip-Form Lining of the San Luis Canal

Author(s): Max R. Johnson

Publication: Journal Proceedings

Volume: 62

Issue: 10

Appears on pages(s): 1313-1326

Keywords: aggregate grading, canal, construction,k contraction joint, lining machine, mix composition, San Luis Canal, slip form paving, trimming machine

DOI: 10.14359/7747

Date: 10/1/1965

Abstract:
Design considerations and construction progress for the San Luis Canal in central California are described. The canal s a principal feature of a large water project being built as a joint effort of the U. S. Bureau of Reclamation and the California Department of Water Resources. It will be over 100 miles long and have an initial capacity of about 13,100 cu per sec when completed in 1967. An unreinforced concrete lining, 4-l/2 in. thick, was selected because of its smoothness and because it allowed a smaller cross section. Experience and economic studies showed that an appreciable saving in capital outlay and maintenance costs could be realized with such a lining. Details of the slip-forming operation, special equipment used, and special joints developed to reduce leakage are described. Concrete mixes and aggregate gradings especially developed for slip-form paving are described.