Bell-Pier Construction, Recent Developments and Trends

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bell-Pier Construction, Recent Developments and Trends

Author(s): Ben C. Gerwick, Jr.

Publication: Journal Proceedings

Volume: 62

Issue: 10

Appears on pages(s): 1281-1292

Keywords: bell pier, bridge, caisson, construction, pier, tremie concrete

DOI: 10.14359/7745

Date: 10/1/1965

Abstract:
The bell-pier scheme of construction is being increas-ingly used for major bridge piers in deep water. This scheme has undergone considerable evolution and improvement in recent years, with better utilization of precast concrete shells, better control and quality for tremie concrete, and improved details which have greatly reduced the amount and complexity of underwater connections. This recent experience portends further developments and use. A number of these trends and potential improvements are suggested for consideration.