Crack Width and Crack Spacing In Reinforced Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Crack Width and Crack Spacing In Reinforced Concrete Members

Author(s): Bengt B. Broms

Publication: Journal Proceedings

Volume: 62

Issue: 10

Appears on pages(s): 1237-1256

Keywords: beam, cracking, crack pattern, crack spacing, crack width, reinforced concrete, research

DOI: 10.14359/7742

Date: 10/1/1965

Abstract:
A simple method is developed for calculation of crack width and crack spacing in reinforced concrete members. The crack widths determined by this method were compared with test data obtained from flexural and tensile members reinforced with one bar. The shape of the main cracks was investigated by means of short tension members of a length equal to the spacing of the main tension cracks. The internal crack formation was determined during loading through injection of resin into a few test specimens. After the resin had hardened and the test members were cut open, the internal crack formation was studied.