Novel Structural Frame Combined With Slip-Form Construction Results in Record Breaking Construciton Time

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Novel Structural Frame Combined With Slip-Form Construction Results in Record Breaking Construciton Time

Author(s): Vincent J. De Simone and Joseph F. Camellerie

Publication: Journal Proceedings

Volume: 62

Issue: 10

Appears on pages(s): 1225-1236

Keywords: construction multistory building, slip forming

DOI: 10.14359/7741

Date: 9/1/1965

Abstract:
The structural frame of a 25-story condominium apart-ment house was constructed in 35 days as a result of com-bining slip-formed bearing walls with precast prestressed floor beams. Construction details, slip-form loads, and floor inserts are described briefly. The use of a climbing crane with its loads, coupled with critical path method, show interesting results.