Behavior of Plain Concrete Under Axial Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Plain Concrete Under Axial Tension

Author(s): Vedat A. Yerlici

Publication: Journal Proceedings

Volume: 62

Issue: 8

Appears on pages(s): 987-992

Keywords: creep, plain concrete, research, tensile load, tensile, strength

DOI: 10.14359/7734

Date: 8/1/1965

Abstract:
The strength and extension of plain concrete under short-time, repeated, and sustained axial tensile load are discussed. Formulas are given to approximate instantaneous and time dependent strain of concrete under constant or variable tensile stress