Control of Rapid Drying of Fresh Concrete by Evaporation Control

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Control of Rapid Drying of Fresh Concrete by Evaporation Control

Author(s): William A. Cordon and J. Derle Thorpe

Publication: Journal Proceedings

Volume: 62

Issue: 8

Appears on pages(s): 977-986

Keywords: concrete, cracking, curing, drying control, evaporation control, evaporation retarder, field application, finishing, fresh concrete, plastic shrinkage, research, shrinkage

DOI: 10.14359/7733

Date: 8/1/1965

Abstract:
Rapid drying on the exposed surface of concrete may result in finishing problems such as stickiness, sponginess, and unevenness; plastic shrinkage and cracking; or a compacted surface which creates a layered structure subject to scaling. These undesirable characteristics may be corrected by control of evaporation with a monomolecular film on the surface of bleeding water. Laboratory tests and field experiences are discussed.