Design of Columns Subjected to Biaxial Bending

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of Columns Subjected to Biaxial Bending

Author(s): John F. Fleming and Stuart D. Werner

Publication: Journal Proceedings

Volume: 62

Issue: 3

Appears on pages(s): 327-342

Keywords: biaxial bending, column, design, tied column, ultimate strength

DOI: 10.14359/7697

Date: 3/1/1965

Abstract:
A simplified ultimate strength method of design for columns subjected to bending about both principal axes is presented. A set of nondimensional design curves for one particular section geometry is given for commonly encoun-tered values of steel percentage, concrete strength, and steel yield stress. The use of these curves is demonstrated by several design examples.