Flexural Failure Tests of Reinforced Concrete Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Failure Tests of Reinforced Concrete Slabs

Author(s): Gene Alan Metz

Publication: Journal Proceedings

Volume: 62

Issue: 1

Appears on pages(s): 105-116

Keywords: cracking, crack pattern, flexural strength, reinforced concrete, research, slab, ultimate strength

DOI: 10.14359/7682

Date: 1/1/1965

Abstract:
Results are presented from tests on 16 small reinforced concrete slabs. Fifteen of the slabs were loaded with a uniequation form load, approximated by a large number of point loads;the other slab was loaded with a concentrated load. Test results are compared with the ultimate failure loads and fail-ure crack patterns as predicted by theory.