Analysis of Circular and Annular Slabs for Chimney Foundations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of Circular and Annular Slabs for Chimney Foundations

Author(s): Kuang-Han Chu and Omar F. Afandi

Publication: Journal Proceedings

Volume: 63

Issue: 12

Appears on pages(s): 1425-1448

Keywords: analysis, chimneys, design, foundations, slabs

DOI: 10.14359/7675

Date: 12/1/1966

Abstract:
Formulas based on the theory of plates are presented for the computation of moments and shears in circular and annular slabs for chimney foundations. The slab is assumed to be of constant thickness, either simply supported or fixed at the chimney wall. Foundation pressure is assumed to vary linearly and exist over all portions of the slab. Results for some typical cases are presented in charts.