Corrosion Effects on Bond Strength in Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Corrosion Effects on Bond Strength in Reinforced Concrete

Author(s): Kyle Stanish, R. D. Hooton, and S. J. Pantazopoulou

Publication: Structural Journal

Volume: 96

Issue: 6

Appears on pages(s): 915-921

Keywords: anchorage (structural); corrosion; cover.

DOI: 10.14359/765

Date: 11/1/1999

Abstract:
Corrosion of reinforcing steel in reinforced concrete affects structural performance in two different ways: by loss of steel section, and through deterioration of steel-concrete bond. In this paper, the effects of corrosion products on bond strength are investigated experimentally. To test the strength of corroded reinforcing bar anchorages and to quantify the effect of deterioration of the bar surface on development length, reinforced-concrete slabs were cast with the ends of the reinforcing bars anchored in the concrete for a known length. Bond breakers were used over the center portion of the bars to control the force demand input to the test anchorage. This measure also served to protect those regions from corrosion. The anchorage zones were corroded to various degrees by applying electrical voltage to the bar ends. Specimens were tested in flexure to assess strength and mode of failure. Results were summarized by means of simple parametric design expressions that relate bond strength to steel area loss.