Measuring the Thickness of a Concrete Slab by Gamma Ray Transmissision

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Measuring the Thickness of a Concrete Slab by Gamma Ray Transmissision

Author(s): Kenneth Preiss

Publication: Journal Proceedings

Volume: 63

Issue: 7

Appears on pages(s): 743-748

Keywords: concrete, gamma ray, measurement, slab, thickness

DOI: 10.14359/7649

Date: 7/1/1966

Abstract:
Describes a method for determining the thickness of a concrete slab by measuring the amount of gamma radiation that passes through it. Results in the laboratory showed that slabs could be measured to an accuracy of better than 2 percent.