Title: Charts for the Working Stress Design of Reinforced Concrete BEAMS

Author(s): B. W. Shirwaikar

Publication: Journal Proceedings

Volume: 63

Issue: 6

Appears on pages(s): 693-700

Keywords: beam;design;doubly-reinforced beam;reinforced concrete;reinforcement;singly-reinforced beam;working stress.

DOI: 10.14359/7645

Date: 6/1/1966

Abstract:
Charts are presented for the working beams in accordance with ACI 31 8-63 stress design The design of singly-reinforced and doubly-reinforced sections is covered by the charts, wherein the amount of tension and compression reinforcement can be read.