Field Investigations of Concrete Bridge Decks in Indiana: Part 2: Detailed Investigation of Existing Decks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Field Investigations of Concrete Bridge Decks in Indiana: Part 2: Detailed Investigation of Existing Decks

Author(s): Lisa M. Samples and Julio A. Ramirez

Publication: Concrete International

Volume: 22

Issue: 3

Appears on pages(s): 59-63

Keywords: bridge decks; corrosion; inspection; plastics; polymers, and resins; protective coatings; reinforcing steels; spalling

DOI:

Date: 3/1/2000

Abstract:
Part 2 of this series reported the results of an extensive field investigation of existing and new concrete bridge decks in Indiana. Initial visual inspections of 114 concrete bridge decks, constructed between 1972 and 1980 were performed. Decks containing epoxy-coated reinforcement (ECR) and uncoated reinforcement were included in the initial field investigation, as well as various other corrosion protection systems. Signs of distress included spalling, areas of delamination, and rust stains. Based on the results reported in Part I of this series, six bridge decks were chosen for a second detailed survey. Part II reports the results of an extensive field investigation of existing and new concrete bridge decks in Indiana. The results from the initial visual inspection of existing concrete bridge decks showed that 46% had signs of distress from corrosion of the reinforcement. Cover measurements were taken on 106 of the surveyed bridge decks. Corrosion of epoxy coated reinforcing steel (ECR) is discussed. Cores were taken for chloride analysis and half-cell potentials on bridges with uncoated reinforcement.