Title: Door Openings in Shear Walls

Author(s): Joseph Schwaighofer

Publication: Journal Proceedings

Volume: 64

Issue: 11

Appears on pages(s): 730-734

Keywords: doors;high rise buildings;multistory buildings;reinforced concrete;research; shear walls;strains;stresses

DOI: 10.14359/7602

Date: 11/1/1967

Abstract:
Describes and discusses a model study of a 22 story high shear wall with three rows of openings. A comparison is made with Rosman’s approximate theory.