Release Agents: How They Work

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Release Agents: How They Work

Author(s): George Baty and Rick Reynolds

Publication: Concrete International

Volume: 19

Issue: 10

Appears on pages(s): 52-54

Keywords: chemical analysis; environments; form parting agents; form removal; sprayed coatings;

DOI:

Date: 10/1/1997

Abstract:
This discussion of the types of release agents used to separate formwork from hardened concrete includes an overview of the chemical properties of the compounds that allow them to work. Practical guidelines on application, with tips on spraying, pressure, and temperature, are provided. Emphasis on the environmental impact concerns with the use of these products is also stressed.