Title: Working Stress Column Design Using Interaction Diagrams

Author(s): George A. Mylonas

Publication: Journal Proceedings

Volume: 64

Issue: 8

Appears on pages(s): 492-498

Keywords: bending;columns (structural);interaction diagram;reinforced concrete;spiral columns;structural design;tied columns;working stress method (structural)

DOI: 10.14359/7579

Date: 8/1/1967

Abstract:
A simplified method for working stress column design is given, by using the interaction diagrams in the Reinforced Concrete Design Handbook, for solving the case of biaxial bending.