Title: Simplified Erection Method for Shell Structures

Author(s): Sylwester Oleszkiewicz and Zbigniew Parniewski

Publication: Journal Proceedings

Volume: 64

Issue: 6

Appears on pages(s): 295-300

Keywords: construction;costs;domes;models;reinforced concrete;reinforcement;research; shells (structural forms);shotcrete;wire cloth

DOI: 10.14359/7567

Date: 6/1/1967

Abstract:
Presents a method of constructing shell structures with the elimination of traditional formwork. Several scaled models were made, including a full-scale dome-shaped shell. The experiments indicate that this construction technique may save over 20 percent of both labor and material costs, with only a slight increase in the amount of steel.