Creep Tests of Two-Way Prestressed Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Creep Tests of Two-Way Prestressed Concrete

Author(s): Howard L. Furr

Publication: Journal Proceedings

Volume: 64

Issue: 6

Appears on pages(s): 288-294

Keywords: creep (materials);lightweight aggregate concretes;losses;prestressed concrete; research;shrinkage;slabs (nonmetallic)

DOI: 10.14359/7566

Date: 6/1/1967

Abstract:
Creep tests on small prestressed structural lightweight concrete slabs are discussed. Three 2 x 2 ft x 2 ‘/2 in. slabs prestressed equally in two directions to 1000, 2000, and 3000 psi, respectively, were gaged for strain. One slab of similar dimensions was prestressed to 2000 psi on one direction. Small 3 x 3 x 1 6-in. prisms were spring loaded axially to the same initial stresses as the prestressed slabs. It was found that creep in the 2000 psi two-way slab was virtually the same as that in the 2000 psi one-way slab. Prestress losses after 313 days were about 25 and 30 percent in the 2000 and 3000 psi slabs, respectively.