Title: Automation on the Job Site

Author(s): Charles J. Pankow

Publication: Journal Proceedings

Volume: 64

Issue:

Appears on pages(s): 281-287

Keywords: concrete construction;equipment;floors;formwork (construction);lightweight aggregate concretes;multistory buildings;panels;placing;precast concrete;prestressed concrete;pretensioning;reinforced concrete;slipforms;

DOI: 10.14359/7565

Date: 6/1/1967

Abstract:
Describes how preplanning between architect, engineer, and builder can provide more economical and efficient construction. The construction of one project where this approach was used is described.