Title: A Yield Criterion for Reinforced Concrete Slabs

Author(s): Rolf Lenschow and Mete A. Sozen

Publication: Journal Proceedings

Volume: 64

Issue: 5

Appears on pages(s): 266-273

Keywords: flexural strength;limit-design method (structural);moments;plastic analysis; reinforced concrete;slabs (nonmetallic);structural analysis;torsion;yield-line method (structural)

DOI: 10.14359/7564

Date: 5/1/1967

Abstract:
A general yield criterion for reinforced concrete plane elements subjected to combination of flexural and torsional moments is developed. The proposed criterion is compared with the results of special experiments devised to test it.