Title: Use of Spiral Welded Steel Tubes in Pipe Columns

Author(s): Noel J. Gardner

Publication: Journal Proceedings

Volume: 65

Issue: 11

Appears on pages(s): 937-942

Keywords: axail loads;buckling;columns (structural);composite construction (concrete and steel);long columns;pipe;reinforced concrete;research;short columns; steels; stresses.

DOI: 10.14359/7525

Date: 11/1/1968

Abstract:
An experimental investigation into the structural behavior of concrete-filled spiral welded steel tubes under axial load is described. The experimental results are compared with the ACI-NBC (1967) requirements, with a previously proposed new ACI-NBC requirement and with the tangent moduli method. Results on the manufacturing stresses in the steel tubes are also given.