Design Procedures for Computing Deflections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design Procedures for Computing Deflections

Author(s): Dan E. Branson

Publication: Journal Proceedings

Volume: 65

Issue: 9

Appears on pages(s): 730-742

Keywords: beams (structural);camber;composite construction (concrete to concrete); cracking (fracturing);creep (materials);flection;flexural strength;modulus of elasticity;moment of inertia;moments;precast concrete;prestressed concrete; reinforced concrete;shoring

DOI: 10.14359/7508

Date: 9/1/1968

Abstract:
Presents design procedures for computing short-time and long-time deflections of noncomposite and composite ordinary reinforced and prestressed concrete beams. The paper discusses phases of the subject indicated in the ACI Build-ing Code but not specifically defined therein, and is, in part, based on recent work of ACI Committee 435, Deflections.