Title: Exploratory Shear Tests Emphasizing Percentage of Longitudinal Steel

Author(s): K. S. Rajagopalan and Phil M. Ferguson

Publication: Journal Proceedings

Volume: 65

Issue: 8

Appears on pages(s): 634-638

Keywords: beams (structural);cracking (fracturing);diagonal tension;flexural strength; reinforced concrete;reinforcing steel;research;shear strength;stirrups;web reinforcement.

DOI: 10.14359/7501

Date: 8/1/1968

Abstract:
The shear strength of reinforced concrete beams as given by ACI 318-63 is known to be unconservative when the ratio of the longitudinal reinforcement, p, is small. The aim of the present investigation was to assess the extent of this inadequacy. Ten rectangular beams without web reinforcement and having p between 0.0173 and 0.0025 were tested; results of 27 other beams with p less than 0.012 from various other investigators were also analyzed. All the beams considered had a/d ratios greater than 2.75. Three rectangular beams with web reinforcement are also reported.