Title: Large Diameter Nonreinforced Cast-in-Place Concrete Pipe

Author(s): Ernest C. Fortier

Publication: Journal Proceedings

Volume: 65

Issue: 7

Appears on pages(s): 544-549

Keywords: cast-in-place pipe;concrete pipe;concretes;construction;costs;equipment; strength;structural analysis;testing.

DOI: 10.14359/7496

Date: 7/1/1968

Abstract:
Describes continuously cast concrete pipe of 72, 84, and 96 in. in diameter. The machinery to produce the pipe is described as are tests and materials of cast-in-place pipe of these large dimensions.