Architectural Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Architectural Concrete

Author(s): James M. Shilstone

Publication: Journal Proceedings

Volume: 65

Issue: 7

Appears on pages(s): 513-515

Keywords: no keywords

DOI: 10.14359/7490

Date: 7/1/1968

Abstract:
A series of papers based on a symposium presented at the 1966 ACI Fall Meeting in New Orleans. The series reviews the special thinking and considerations required for architectural concrete which must be structurally sound, aesthetically pleasing, and as economical as possible. The papers view the subject from the standpoint of architect, engineer, and builder. Following a brief introduction, four authors cover, in turn, the architect’s approach, structural implications, planning requirements, and construction.