Title: Reccommended Practice for Concrete Formwork (ACI 347-68)

Author(s): ACI Committee 347

Publication: Journal Proceedings

Volume: 65

Issue: 7

Appears on pages(s): 497

Keywords: aggregates;aluminum;anchors;architectural concrete;bridges (structures); buildings;canal linings;civil defense;coatings;composite construction; concretes;construction;construction materials;culverts; drawings;falsework; fiberboard;folded plates.

DOI: 10.14359/7487

Date: 7/1/1968

Abstract:
Presents brief introductory statement on the need for formwork standards based on the fact that 35 to 60 percent of the total cost of the concrete work in a project in the United States is in the formwork. A section is given on engineer-architect specifications noting the kind and amount of specification the engineer or architect should provide the contractor. Since the committee concludes that formwork design and engineering, as well as construction, must be the responsibility of the contractor, the recommendations contained in the report are directed to that group. However, an understanding of these recommendations by engineers and architects will aid these groups in their specification functions. The report is divided into five chapters: 1. Design, 2. Construction, 3. Materials for Formwork, 4. Forms for Special Structures, and 5. Formwork for Special Methods of Construction.