Componets of Creep in Mature Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Componets of Creep in Mature Concrete

Author(s): J. M. lllston

Publication: Journal Proceedings

Volume: 65

Issue: 3

Appears on pages(s): 219-227

Keywords: beams (structural);bending;continious beams;flexural strength;reinforced concrete;shear;stirrups;stresses;torsion.

DOI: 10.14359/7469

Date: 3/1/1968

Abstract:
Tests are reported on the creep and recovery of concrete under uniaxial compression and tension, applied at ad-vanced ages of over a year. The characteristics of the creep components (irrecoverable or flow, recoverable or delayed elastic) for young and mature concrete are compared, and found to be in reasonable agreement. The rate of flow method (based on the two components) for calculating strain under variable stress is discussed. In particular, it is compared favorably with super-position.